< Home
 
Product profile (Grades)
 
 
BUTYL RECLAIM
BT 999
 
 
Source
   
   
Butyl automobile tubes.
     
 
Specification
     
Chemical Properties
 
Ash%
4 ± 2
Carbon Black %
32 ± 4
Acetone Extract%
9 ± 3
RHC By Difference%
50 min.
     
Physical Properties
 
Specific Gravity%
1.14 ± 0.02
Tensile Strength kg / cm²
75 min.
Elongation @ Break %
480 min.
Mooney Viscosity
ML (1+4) @ 100°C.
30 - 45
Hardness at Shore A
51 ± 3
     
 
Advantages

  • Faster Mixing Cycle ie. Less masticating with easy incorporation.
  • Improved extrusion rate.
  • Improved extrusion quality with better control on dimensions.
  • Reduction in splicing defects.
  • Reduction in electrical power consumption due to less nerve of the compound and faster mixing and extrusion.
  • Minimum increase of air permeability as compared to other grades of Reclaim Rubber.
  • No reduction in hot air aging properties.
     
 
Applications
   
   
  • Butyl inner tubes.
  • Tyre inner liner.
  • Adhesives.
     
 
Recommendation
     
   
Application
Max PHR
Butyl Inner Tubes
20-30
Tyre Inner Liner
20
Adhesives
30
Cable beading
60
Sound dampner
50